    Hi,

    I have been using Caswell's buffing wheels and rouges for an exceptional shine on my sterling and plated silver. One thing I have not been able to accomplish is how to buff the inside of spoons to the same lustre due to the small concave shape. The wheel will not go down into the bowl of the spoon. Does anyone know of a solution? I have to manually polish the spoons which is very time consuming and does not give the same results. I have tried a small felt bob on a drill but it did not work.

    Any help would greatly appreciated.

    Thanks,

    David

  • #2
    you need to get a mop buff to do the inside... i think caswell sell's them. if they don't have it on there webpage i am sure they can get it or they may stock it

    Comment


    • #3
      PROD SMW400 Shank Mounted Wheel 2" Dia x 1/2" Thick x 1/4" Shaft $4.50

      PROD SMW450 Shank Mounted Wheel 3" Dia x 1/2" Thick x 1/4" Shaft $5.00
      --
      Mike Caswell
      Caswell Inc
      http://www.caswellplating.com
      Need Support? Visit our online support section at http://support.caswellplating.com

      Comment


      • #4
        i thought they did but i was not sure

        Comment

        Working...
        X
        😀
        🥰
        🤢
        😎
        😡
        👍
        👎