Announcement
Collapse
No announcement yet.
What is the best way to polish magneseum?
Collapse
X
-
Guest repliedit is a sealer protector ... caswell stock's it it cos a lot but it save's you from polishing every few months and last a year
-
Guest repliedpolish it as if you were polishing alum. and then you can coat it with zoop or high grade carnuba wax ....
Leave a comment:
-
What is the best way to polish magneseum?
I hane a supercharger that is made out of magneseum. I can polish it with metal polish, but it dosen't stay shiny very long. It starts to tarnish within a few days. Is there anything out there that can polish magneseum, and stay shiny? Can I coat it with something?
Thanks, JimTags: None
Leave a comment: