  • bead blasting powder coat ??????

    I need to remove powder coating from alloy wheels super fast ,Can anyone tell me what media is hands down the fastest with out disturbing the base aluminum ( too Much ) final process is polishing. Thanks in advance..................... John

  • #2
    take them to a machine shop and have them steel shot for a few bucks and you will be set

    Comment


    • #3
      Quick question on that , How long does it take to steel shot a powder coated wheel completely clean, and wont steel shot disrupt the aluminum/alloy surface? Thanks

      Comment