there is a post on here from nautishine back aways that tells you from start to finish on how to do a frame its really great and kinda entertaining. hope it helps clydes
-
polishing ?
alright so i used a scotch pade 4in round on my die grinder to remove the finish on the alum, then i sanded some and so i moved on to polish so i used some red rouge then when i went to white, it would turn black in spots and some spots looked almost pitted not really shining out then when iu cleaned off the rouge it still looked kinda pitted, is this common, did i just need to keep o nbuffing to get it out? i thought it was not prepped good enough and went back and am re-sanding right now and being more carefull, need some help please?Tags: None