What part of the wheel do you actually use to polish? I have been using the outside edge of it to do my polishing, is this correct? Should I be using the face instead? I would think it difficult to load up the face of the wheel.
Announcement
Collapse
No announcement yet.
What part of the wheel
Collapse
X
-
Re: What part of the wheel
You use the outside edge of the wheel, as you have been doing.
You might want to read our free buffing booklet at http://www.caswellplating.com/buffman.htm--