    I noticed some oxidation on a few parts I recently buffed and installed on my bike. I did some searching on the web and one online retailer stated that carnauba wax was acidic therefore speeding up the oxidization process. I figured it was just another way to endorse their product so I did some Google'n. I found that not only will acids harm aluminum, so can alkylines, and that only neutral compounds should be used. That's about as far as I've gone with my search so far. What do ya'll think? I'll do some more searching and see what else I can come up with.

    Steve

  • #2
    thats why zoopseal is the best choice out but it is pricey
    when in doubt polish it out/ why replace it when you can refinish it
    G2 Polishing and Powdercoating

    Comment


    • #3
      Nope .. you need to use high grade carnuba wax not the stuff you buy in the autoparts store. you want top of the line. most waxes on the market have water in them that is where you are having problems . i use the same carnuba wax on my parts that i ship out that i use on high dollar cars never had any problems at all

      Comment


      • #4
        customandsound,
        Who deals the high end carnuba wax? Is there a specific brand?

        Comment


        • #5
          Originally posted by sswee
          customandsound,
          Who deals the high end carnuba wax? Is there a specific brand?
          Ah yes, the $1,000,000 question.

          Comment


          • #6
            i get my wax from a detail supply house.. caswell sells some top of the line waxes to check with them if all else fails go to the local autobosy shop and sneak a peak at there bottles and offer to purchase a little from them ..

            Comment


            • #7
              Thanks for the info bro. I think with that I can find the stuff I need. Later on.

              Steve

              Comment


              • #8
                Thanks for the info bro. I think with that I can find the stuff I need. Later on.

                Steve

                Comment


                • #9
                  no problem .. glad i could help