    Chuck..I have heard that using steel wool will load up in the aluminum making the tiny bits of steel that got imbedded rust over time...I haven't seen it yet, but just throwing some info your way!...LOOKS GOOD!

    Leave a comment:


  • Guest's Avatar
    Guest replied
    the valve cover .. I glassed beaded Grease less then took a sprial with black tore it up. the recess's i use felt bobs and facer buff's on a air die grinder ...

    with the glass bead you can get away with a quick polish the total time on that valve cover from raw to done around 1/2 hr...

    Customer paid 70.00 to have it done .. that pic don't help it any. i took it with a cheap camera ...

    Leave a comment:


  • turbohardtop
    replied
    What did you use to polish the "half-circle" concave part. I have similar cut out shape on my Supra valve covers.

    Leave a comment:


  • Guest's Avatar
    Guest replied
    yep i did the powder to .... i tryed to pack up all my polishing stuff but i i got it in my blood. i just could not let it sit there any more

    here is another :

    Leave a comment:


  • easleysp
    replied
    Great job on a cool looking wheel. Pick, money talks brother, even for a pro. Later on.

    Steve

    Leave a comment:


  • pickleboy
    replied
    dang chuck that is shiiiiiney. the powder looks good too did you do that as well? i thought you got out of the polish game?

    Leave a comment:


  • fly
    replied
    Looks good from here.

    Leave a comment:


  • Guest's Avatar
    Guest started a topic a few polished parts Better than chrome !!!

    a few polished parts Better than chrome !!!

    what ya think?

    All the polishing was done by hand



    i uses 0000 steel wool and firtz polish i got a sample from caswell a while back ..