I am thinking of picking up an air die grinder. Which one is more comfortable to work with...90 degree angle or straight? Thanks.
Announcement
Collapse
No announcement yet.
die grinder...right angle or straight
Collapse
X
-
The 90 if your using the disk type (3Mpads), but I suggest both so you can use the flappr wheels also, you find that they both are useful in the plating business.
-
Re: die grinder...right angle or straight
The angle is for the 3m disk not the flapper wheels. You don't have to get a expensive grinder, just keep it oiled and by the way you can buy two grinders for one of the big name grinders. Unless you just have the money buy the big name brand, but when your on a budget you have to do what can to get by, trust me I know.