Guest repliedremove clear coat. wet sand with 1500-2500 grit then use a wax or metal polish to bring the shine right back to par...
-
Caswell has an aluminum finishing and polishing kit that has everything you need except the sealer for after you polish them.
http://www.caswellplating.com/buffs/alwheel.htm
Leave a comment:
-
Aluminum Wheels - What do I need?
I just bought some used Aluminum Wheels and I want to polish them.
Please tell me what I will need (products/wheels/compounds) to polish them.
thanks[/img]Tags: None