Guest repliedRe: Greaseless Coumpounds
Rule of thumb 1 wheel pre... you can clean them good but chances are you will not get all the 80 grit out and so on.....
Leave a comment:
-
Re: Greaseless Coumpounds
You still need different wheels for different grit compounds. They are the same as other compounds, just in a different media.
Leave a comment:
-
Greaseless Coumpounds
Is it ok to use one wheel for muliple greaseless coumpounds?
i know the answer for the polishing compounds where you need one wheel per compound.
thank you.Tags: None