caswell has a felt bob kit which you can use with your dremel and some greaseless compounds. They will be even faster that the paper.
Good Luck!
Leave a comment:
-
ok great! I will order some up right away!What do i use for the recessed area once i rid the piece of the casting marks? I had mentioned the dremel but
If the dremel is what i need to use won't if give me a different final finish? What i mean is i am using the wheel on the most of the piece and in that particular area the wheel won't fit.
Leave a comment:
-
Cutting Faster
You need to use Wet and Dry Paper to remove the casting marks. See http://www.caswellplating.com/wetanddry.htm
Once the casting marks are gone, move on with the black compound.
Leave a comment:
-
What will cut this faster?
I am polishing my turbo housing on my truck. As you can see in the picture the housing is really rough. I am using an 8" spiral sewn cloth wheel and the black compund spining at 3150rpm's. That little bit that is shiny took me like a 1/2 hour.There must be something better. Also what can i use to get in the area that is recessed around the intake part of it? I have not used the dremel. Will that be my tool? Anyway what can be used to spped this up?