Just thought I'd share this with ya'll.
I made some felt wheels to use with greaseless compound the other day using a hollow punch set (2" x 1/4") and some felt material we have at work. I also punched some wheels out of a few scotch brite pads, but they're a little on the flimsy side. The felt wheels worked pretty good with greaseless though.
Steve
I made some felt wheels to use with greaseless compound the other day using a hollow punch set (2" x 1/4") and some felt material we have at work. I also punched some wheels out of a few scotch brite pads, but they're a little on the flimsy side. The felt wheels worked pretty good with greaseless though.
Steve