Just wondering if anyone has tried prepping stainless with greaseless before polishing
Announcement
Collapse
No announcement yet.
stainless & greaseless
Collapse
X
-
Re: stainless & greaseless
this i have done i used 400 grit on a piece of mill finish with small scratches from the tooling. it worked great to get it smooth. then on to sisal and fast cut stainless bar. vented emory and then spiral and green, then spiral and white.when in doubt polish it out/ why replace it when you can refinish it