    For others reading this, use Anodize Stripper.

    See http://www.caswellplating.com/aluminum.htm

    Leave a comment:


  • rotorman
    replied
    please ignore - I've just found the answer to my question doing a search.

    sorrry!

    Leave a comment:


  • rotorman
    started a topic removing anodizing for polishing

    removing anodizing for polishing

    I just bought an oil filler cap made of solid aluminium. I want to polish it but it has an anodised red finish that I can't seem to remove.

    SAnding works, but the layer is so tough it will take forever. Paint stripper don't work either.

    I've been told to use oven cleaner on the part?

    Any other suggestions.