    totally new to the stuff..

    is there a way to trun what is already chromed stuff into shadow chrome..

    do you have a product that does that?..

    what exactly is shadow chrome anyway.

    TIA

  • #2
    Shadow Chrome = Black Chrome

    It's a different chemical process than regular chrome. You can't turn regular chrome into black chrome.

    We don't supply a black chrome product.
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com

    Comment


    • #3
      Re: shadow chrome / black chrome

      Is Shadow Chrome and Black Chrome the same thing?

      Comment


      • #4
        Re: shadow chrome / black chrome

        No, there is actual black chrome, which is a very dark chrome as Caswell is alluding to ^ I'ts proper plating and I don't know how they do it.
        And then there is a paint finish, shadow chrome, which is a black base with a special silvery coloured clear coat over the top of it, what you see on many car wheels