I'm polishing some aluminum windshield brackets on my motorcycle and have a couple questions. Not sure what type of aluminum they are.
First, I am using black compound to get a fairly decent shine and then I switch to brown to finish them. I am not getting a mirror finish like I'm wanting. Do I possibly need to use white to get them to shine or is it maybe just the metal and I'm getting the best finish possible ? I am using a 3/4 hp 3450 rpm bench mounted motor. The wheels are an 8" sisal with the black compound and an 8" sewn wheel with the brown.
Second, when I'm finished polishing them and I try to use a polish (Mother's - Blue Magic) I get a bunch of little scratches. They are easy to see, although they are not real deep. Even just wiping them with a clean rag makes small scratches. Do I need to use some sort of cleaner first ? I have tried kerosene first, but that seems to make no difference.
Any help with these problems would be greatly appreciated. These are my first attempt at polishing and I'm sure it's just something that I'm doing wrong !
First, I am using black compound to get a fairly decent shine and then I switch to brown to finish them. I am not getting a mirror finish like I'm wanting. Do I possibly need to use white to get them to shine or is it maybe just the metal and I'm getting the best finish possible ? I am using a 3/4 hp 3450 rpm bench mounted motor. The wheels are an 8" sisal with the black compound and an 8" sewn wheel with the brown.
Second, when I'm finished polishing them and I try to use a polish (Mother's - Blue Magic) I get a bunch of little scratches. They are easy to see, although they are not real deep. Even just wiping them with a clean rag makes small scratches. Do I need to use some sort of cleaner first ? I have tried kerosene first, but that seems to make no difference.
Any help with these problems would be greatly appreciated. These are my first attempt at polishing and I'm sure it's just something that I'm doing wrong !