    I went about cleaning a piece of aluminum the usual way with some hot simple green and water and I had a thought. I used one of those Mr Clean magic eraser sponges in the kitchen the other day and I was kinda impressed with it. Figured why not give it a try on some buffing compound. Worked like a champ! And no scratches!

    Steve

  • #2
    Re: It really is magic!

    What did you do ??
    use it with compound ?

    Comment


    • #3
      Re: It really is magic!

      I used it to clean the compound off the part. I usually use a flannel cloth to clean areas where any compound built up. Just figured I'd give the magic sponge a try and it worked. Cleaned 'er right up!