on my harley I want to turn all my beautiful chromes into a mat/satin finish ,no more shine.Is there a chemical gentle enought that would do that without having to recoat to prevent rust.thank you for your time.
Announcement
Collapse
No announcement yet.
from nice chrome to satin
Collapse
X
-
You'll need to strip the existing plating, bead blast the part to a satin finish, then re-apply the plating.--
Mike Caswell