  • chrome look

    alright ive recently got everything done and im starting to rebuild my bike my question is some of my parts have been chrome plated i.e brake pedel,heel guards,foot rest mounting brackets small stuff. and my frame i polished, when you look at the frame thers no scratches in it but it looks to be a differnt color or clearness in the reflection compared to the plated parts. why is this and can you get the polished part to look like the plated parts

  • #2
    Aluminum is going to have a brighter shine than chrome. Different grades will shine differently.

    Comment


    • #3
      thx

      Comment


      • #4
        chrome plate the aluminium and it will look the same.

        Comment


        • #5
          i think he means it has that spiderweb scratch hazy thing going on tha makes it look a bit dull when looked at a different angle... right?