    i need help with instructions on polishing the aluminium on my 2001 suzuki
    gsxr600. what i need to know is the correct grits of sandpaper to buy and a step by step walkthrough to get the job done.

  • #2
    ...

    Buy the following: A tube of 240grit greaseless, large bar of black compound, large bar of brown compound, three spiral sewn wheels, and an arbor adapter.

    Use the greaseless...
    Use the black compound...
    Use the brown compound...
    Clean it up with flitz.

    It's not hard... but your making the same mistake I did. Starting after the start of riding season. Good luck!