I just wanted to get an idea of what kind of tools everyone uses for their polishing. I am looking for something small and handheld that can polish my rims. Thanks
Announcement
Collapse
No announcement yet.
Polishing Aluminum Wheels
Collapse
X
-
A drill and 4" wheels are probably the most common tool.
See http://www.caswellplating.com/buffs/alpolkit.htm--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com