Can Electroless Krome be applied to a zinc die cast part? If so, what is the procedure?
Announcement
Collapse
No announcement yet.
Electroless Krome on zinc
Collapse
X
-
Electroless nickel cannot be applied to a zinc part. You must PRIME the pot metal with either 'Electroless Pot Metal Primer' - an electroless nickel that is alkaline, or Flash Copper.--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com