    i have several pieces of 440 stainless steel which were blackened from submersion in a lime-away type fluid. can anyone offer a solution for removing the resultant blackening from the stainless?

  • #2
    Re: how do i remove blackening from stainless?

    Try a 20% solution of muriatic or hydrochloric acid.
    --