    I've used the black oxide gel on carbon steel and while it works well, the sealer goes on with a lot of bubbles and will not dry smoothly.

    Am I doing something wrong? I am brushing the sealer on to the dried product with a paintbrush. The bubbles consistently form and when dried overnight remain, leaving an uneven finish.

    Any help would be appreciated.