    Question, aside from knives and the like, is anyone doing a deeper electro etching in brass, copper, or silver? I am trying to use this as a way to deeply (.2mm or more) etch patterns into jewelry we make. I usually use mordents like ferric chloride and nitric acid. I hate using those chemicals Would rather use electro etching (uses friendlier chemicals which are not exhausted by the etching process). I have done 4 test runs so far using copper, and am having some issues I would like to discuss on here if anyone has refined the process. TNX!