  • Copper immersion

    Hey don't know where the appropriates spot to post this is but have a question. I've been a plater for quite awhile now. Here the question. I was derusting my motorcycle gas tank. I used vinegar and copper plated copperhead BBs. Now that all the rust has been removed the vinegar stripped the copper off the BBs and now I have copper immersion inside the whole tank. what's the best way to remove this with out destroying the tank? What will strip the copper out of the tank with out compromising the inside surface area? Thank you.

  • #2
    Were you cleaning it to use tank sealer ? or to plate the tank ?
    --
    Jason Vanderbroek
    315 946 1213 x116
    www.caswellplating.com