    Can the Caswell Cobalt plating kit be used directly on stainless steel? I have a stainless steel Glock pistol slide that I would like to cobalt plate.
    Look for this. Stainless steel Activator
    STAINLESS STEEL ACTIVATOR - 8OZ - Caswell Inc (caswellplating.com)‚Äč

    If you need a larger than 8OZ you will need to look into what's called woods nickel strike(acidic Nickel Chloride bath), lays a nice Nickel layer ontop of Stainless Steel so other metals like Cobalt can be plated ontop.

    Leave a comment:


  • Ethan Connor
    replied
    Yes i think, you would need to plate with copper first then Cobalt.

    Leave a comment:


  • Caswellplating_Jason
    replied
    dc please call us at 315-946-1213 xt116 and we can trouble shoot with you.

    Leave a comment:


  • dc
    replied
    Having issues with lowers with black finish coming out marbled, can anyone help me ?

    Leave a comment:


  • Caswellplating_Jason
    replied
    You would need to plate with copper first then Cobalt.

    Leave a comment:


  • Rustynuts72
    started a topic Cobalt plating stainless steel

    Cobalt plating stainless steel

    Can the Caswell Cobalt plating kit be used directly on stainless steel? I have a stainless steel Glock pistol slide that I would like to cobalt plate.