Hi, just used the kit and it works Great!
One thing I did get first time was
When I put the lacquer on The finish
turned a little gold in color?
I used the same gun I used for the sensitizer
I ran Thinner though the gun to clean it before putting in
the Paint ,would just a slight bit of
Sensitizer in my gun contaminate my top coat
and make it turn the gold color?
I noticed the Lacquer has a slight Amber tint to it.
Thanks Jdee