Guest repliedwhen i buff out my painted and powder coated parts i use carnuba wax it makes them shine.
-
thanks
My buffing whells will run at 860rpm. Do you spread the glaze on the surface or do you "soak" the flannel wheel with the glaze?
Thanks a lot.
Eric
Leave a comment:
-
The liquid glaze will work. It's what I use to use on auto paint work. It will probably be a little messy. Be careful not to burn the coating. SS
Leave a comment:
-
3M Liquid Glaze Compound with Flannel Wheels?
Hi,
I am trying my new polishing arbor. I am planning to use a flannel buffing wheel in order to bring my drum shells to a high luster. The clear coated was sanded up to 2000 grit. Can I use 3M liquid compound to achieve it? Or do I actually need to use dry compound?
Thanks,
EricTags: None