    what product can be used to blacken springs that have been zinc coated??

  • #2
    Re: Blackening over zinc plating

    Black Chromate or Zinc Blackener (an oxide).

    Chromate has much better corrosion resistance, and is more durable.
    Seans Zinc Plating page