  • Recommendations for muffler paint?

    I would like to change the color of the factory muffler on my 2001 Acura CL Type S. It is currently a flat black finish with dull-looking chrome tips. I would like to change the color of the whole muffler (including tips) to a silver or brushed aluminum look.

    Which of your high temp spray paint products would you recommend?

    Thanks,
    Mike

  • #2
    Re: Recommendations for muffler paint?

    We recommend the VHT Flameproof coatings for this application.

    See <a href=\"/vht_high.htm\">our VHT Page</a>.
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com