Anodized a bar of aluminum yesterday. Anodizing went perfectly. However, first time using the Olive green dye and it came out copper colored, burnt orange; not a spec of green in it! Is it possible the dye was mislabeled or is there some other issue? I can live with the color, but don't want it to happen again. Any suggestions?