  • Black Oxide

    Can you use that on Al?

    Thanks,
    Ben

  • #2
    No, just steel (not stainless)

    We have a chromate for aluminum that gives a yellow/brown color. See http://www.caswellplating.com/aids/metal.htm

    Your other option is anodizing.
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com

    Comment


    • #3
      Can you recommend any places for anodization?

      Thanks,
      Ben

      Comment


      • #4
        We recommend you do it yourself. See http://www.caswellplating.com/kits/aluminum.htm
        --
        Mike Caswell
        Caswell Inc
        http://www.caswellplating.com
        Need Support? Visit our online support section at http://support.caswellplating.com

        Comment


        • #5
          ok, ok, i geuss you wont tell me.. dont wana loose any buisness.

          But im just in HS and have no clue what im doing... how hard would it be...

          Oh and why cant things be anodized white? what is the lightest possible color things can be anodized?

          Thanks,
          Ben

          Comment


          • #6
            It's not that we don't want to tell you, we just don't know of any places because we've never had the need to have anyone anodize something.

            You can't anodize white because the dying process is semi-transparent. If you dyed something white, the grey aluminum color would show through, making a grey color.

            The lightest color is probably a light grey.

            Why don't you talk to your science teacher and see if he's interested in experimenting with a kit. We sell quite a few kits to science teachers in High School for class demonstrations etc.
            --
            Mike Caswell