    I am having problems with some of my parts. I stripped them as instructed, and when I put it into the Desmut, it makes a white coating on the part. When it goes into the anodizing tank, it turns black or grey, and i gotta start over. Am I doing something wrong? How can i get it back to bare aluminum besides buffing?

    Otherwise things are going good!

    Robert Walker

  • #2
    Is anyone from Caswell going to reply?

    Comment


    • #3
      Please post a problem report in our tech support section. We'll post an answer for you within 24 hours.

      Thanks
      --
      Mike Caswell
      Caswell Inc
      http://www.caswellplating.com
      Need Support? Visit our online support section at http://support.caswellplating.com

      Comment


      • #4
        Re: Buildup after using Desmut

        You need to thoroughly rinse the part before going into the anodizing tank.
        --
        Craige Brooks
        Caswell Inc
        http://www.caswellplating.com
        Need Support? Visit our online support section at http://support.caswellplating.com
        Have A Web Site?
        Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm

        Comment

        Working...
        X