Re: Buildup after using Desmut
You need to thoroughly rinse the part before going into the anodizing tank.
Announcement
Collapse
No announcement yet.
Buildup after using Desmut
Collapse
X
-
Please post a problem report in our tech support section. We'll post an answer for you within 24 hours.
Thanks
Leave a comment:
-
Buildup after using Desmut
I am having problems with some of my parts. I stripped them as instructed, and when I put it into the Desmut, it makes a white coating on the part. When it goes into the anodizing tank, it turns black or grey, and i gotta start over. Am I doing something wrong? How can i get it back to bare aluminum besides buffing?
Otherwise things are going good!
Robert WalkerTags: None
Leave a comment: