I purchased this product to fill a gouge in an anluminum mag wheel.
I can not get it to melt. I have tried a propane torch and a butane torch. It seems to start to melt and then does nothing. After it cools it just wipes off.
If I try it on an eighth inch thick aluminum bar it melts and beads to a ball. I thought it would flow.
Am I doing something wrong or just not enough heat from the butane (it is supposed to go the 3100').
Thanks
Terry
I can not get it to melt. I have tried a propane torch and a butane torch. It seems to start to melt and then does nothing. After it cools it just wipes off.
If I try it on an eighth inch thick aluminum bar it melts and beads to a ball. I thought it would flow.
Am I doing something wrong or just not enough heat from the butane (it is supposed to go the 3100').
Thanks
Terry