    I am preparing to refinish several sets of golf club irons that are made of 1025 carbon steel and chrome plated. I want to refinish them with the black oxide finish.

    Is this finish durable enough for a golf club?

    Will the finish chip or fade easily?

    Does anyone have any suggestions for this project?

    Thank you in advance for any assistance you can provide.

  • #2
    Re: Golf club refinishing with black oxide

    it is durable enough for a golf club, but if not properly maintained it will rust and chip

    Comment


    • #3
      Re: Golf club refinishing with black oxide

      Will the cold black oxide treatment wear off on the sole of the club?