    I'm planning to a anodize an aluminum PC case, but have a few steel and brass parts that are embedded into the aluminum.
    I've recently purchased a can of Mask-It to spare these bits from the acid, but would like to know, what would be used to strip the mask off afterwards without harming the anodized coating?

    I'm trying to anticipate every problem before-hand so this project won't drag on forever.

  • #2
    It should peel right off, like rubber cement.
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com

    Comment


    • #3
      Thanks, that's reassuring.
      I'm taking pics of the project as I go, and I'll try to remember to post at least a link to them once complete. Great resource for metal finishing, even for a 'noob', Thanks again.