    Hello. I currently do small scale commercial titanium anodizing. In trying to meet customer demand for more available colors and better consistency I'm looking into using a dye based anodizing system rather than the refractory anodizing more commonly used for titanium.

    My specific question today is wether the anodizing dyes sold here at Caswell will dye anodized titanium as well as aluminum and if not what alternatives are there?

    Also if anyone has any insights or experiences with this type of process please feel free to share them, any info is appreciated. Thanks.

  • #2
    Our dyes will not work on titanium.
    --