    Do any special cleaning or surface preparations have to be made for coating aluminum or fibreglass. What is the lowest temperature the powder coating material cures at and is still durable. Thanks

  • #2
    Re: Aluminum and Fibreglass Coating

    Ideally, a metal surface should be sandblasted

    You can't powder coat fiberglass, the cure temp is far too hot.

    Temps for curing vary depending on the actual coating color, so we cover it
    all with 450 f
    --
    Mike Caswell
    Caswell Inc