    replied
    Re: powder coating stainless steel

    Originally posted by DALE
    Are you sure it outgassed? Usually stainless doesn't outgass, it does however have poor conductivity making it difficult to get sufficient powder on the surface.
    so, how does one go about coating SS? blast, clean, then phosphate? how do you get around the conductivity issue? i have a project to coat SS and end up looking like translucent anodized aluminum ... i'm going to try some things, any suggestions here sure would save some time.

    Leave a comment:


  • DALE
    replied
    Are you sure it outgassed? Usually stainless doesn't outgass, it does however have poor conductivity making it difficult to get sufficient powder on the surface.

    Leave a comment:


  • chevellenut
    started a topic powder coating stainless steel

    powder coating stainless steel

    did anyone coat stainless steel is have it come out looking good without any outgassing?..i tried it a couple time with the same outcome "ugly" .
    i sand blasted it scuffed it with sand paper cleaned it with thinner baked it for 30 min powder coated it after it cooled and cured it for 30 mins at 350 degrees. and i tried to coat it a second time as soon as it came out of oven only to have it look the same any suggestions..thanks for your time