What your oppion? I was thinking of a 1500 IR light but after breezing through the posts it seems to be a waste of money.
Announcement
Collapse
No announcement yet.
IR light or electric oven?
Collapse
X
-
It all depends on your application,bud. Personally....from the things you say you want to do, I'd go with the IR lamp. You can always find a cheap if not free electric oven down the road for doing more specific things. I doub't you'll find one to fit a transmission case in though,lol. IR will suit your purposes (now and future) just fine. ....Russ