I need to know if thier is a limit to the size of metal that is being coated. I am building a bake oven that is 4ft wide by 3ft deep by 8ft tall with divider panels in it for use with smaller parts, so that I can coat my car chassis. I would hate to go through all this work and find out my hobby gun will only do a small part.
Announcement
Collapse
No announcement yet.
is thier a size limit
Collapse
X
-
exactly.... you have no size limit. Mush as one wouldn't have any limitations on a liquid set-up either. Just because you are usung a "hobbyist" gun doesn't mean you are limited to small parts. If your hobby is coating car frames, then so be it! I've said it before and I'll say it again.... the only limitation is your imagination! Good luck and PLEASE.... post a pic when yer done (sorry.... I love seeing pics of what you guys do. Makes me feel all warm and gushy inside,lol). Keep us posted,k? Russ