I've done a few magnesium parts in the past and got good results. A customer is sending me an expensive motorcycle engine block that has been vapor blasted. He wants me to PC it in a clear satin finish to protect it. I don't expect any issues, but wanted to ask here just in case anyone has advice. I will do my usual wash/dry/outgas before I begin masking for powder.
Thanks.
Thanks.
Comment