  • Anti flash coating for ferrous- after blasting.

    Been researching in circles.....after sand blasting I am looking for a spray/mist on pretreatment that will halt oxidation without the need for further washing on steel/iron prior to zinc powder and powder coating. I have found Bonderite/Henkel 1201 for aluminum. I think Picklex is way over priced and looking at Ospho or locally brewed FlashGuard. My list is limited due to availability and or shipping. Open to other choices that are thin enough to spray.

    http://www.guardianchem.ca/Products-Ser ... HGUARD-NLB

  • #2
    Zinc plating will not occur over any of theses Coatings.
    --
    Jason Vanderbroek
    315 946 1213 x116
    www.caswellplating.com

    Comment


    • #3
      Powder coating over surface conversion coating. No plating.