    This is my first day here and only second post, so I figured pics would come next. I have a small area right now but have been happy with the results to date.


    I want to build a spray booth and a larger oven very soon.

    Kevin

    Comment


    • #32
      Sorry about the size

      Please forgive me.

      Comment


      • #33
        Hi,

        I just started powder coating a few days ago. I'm trying to restore a 48 1.5 ton Chevy. I just put together an inexpensive spray booth you can take down or set up in just a few minutes.
        I used PVC pipes slid into each other (no glue) and 4 mil. painters plastic drop cloth to cover. The table and base is an old garbage can which has a box fan on top for ventilation blowing down and dryer tubing at the bottom of the can to vent the dust out. The filter is on the fan also serving as a table top. At the top of the booth I have a 1x6 with three hooks which hold my projects. All three hooks are connected by grounding wire and I just hook the grounding clip to the wire thus enabeling me to do 3 items at once if needed. I will try and get some photos.

        Aloha,

        Keoni

        Comment


        • #34
          Pictures of my setup

          My home made booth, foil covered foam board, an A/C filter and an old vent-a-hood.


          My home made 6'X3'X3' electric oven.


          I also have a blasting cabinet from one of the popular cheapy tool companies.
          Lee Parsons
          Rowlett, TX (East Dallas)

          Comment


          • #35
            Re: Pictures of process and equipment

            My Shop pics. Not much but it works. Been getting it setup since October '05.





            Last edited by cdaeme; 01-31-2006, 08:47 PM.

            Comment


            • #36
              Re: Pictures of process and equipment

              More......




              Comment


              • #37
                Re: Pictures of process and equipment

                More......





                Comment


                • #38
                  Re: Pictures of process and equipment

                  More.......




                  Comment


                  • #39
                    Re: Pictures of process and equipment

                    More.....





                    Comment


                    • #40
                      Re: Pictures of process and equipment

                      More.....



                      There is also a '66 Mustang Coupe on the backside of the blue curtian.

                      Jason Williams
                      Auto-Cycle PC
                      Chattanooga, TN
                      Last edited by cdaeme; 01-31-2006, 08:50 PM.

                      Comment


                      • #41
                        Re: Pictures of process and equipment

                        very nice shop space there bro.
                        when in doubt polish it out/ why replace it when you can refinish it
                        G2 Polishing and Powdercoating

                        Comment


                        • #42
                          Re: Pictures of process and equipment

                          I can't see any pics on the 1st page....just red Xs
                          Last edited by JeffL; 03-07-2006, 07:44 PM.

                          Comment


                          • #43
                            Re: Pictures of process and equipment

                            I cant see most of the pics, but thats probably because Im at work. Damn blocking software.

                            I agree DONT USE PLAYSAND! Ive read alot about silicosis, nasty stuff. To the person in Orlando, FL . Tractor Supply Stores sell glass bead and aluminum oxide. Its not that expensive if your not blasting to waste.

                            Comment


                            • #44
                              Re: Pictures of process and equipment

                              started with a caswell gun, worked my way upto a Nordson Sure Coat gun.


                              Home built 8wide8high13long oven.

                              got the little guy stile there also. old hoome oven still too..

                              http://www.cecoatings.com/images/coa...0In%20oven.jpg

                              Comment


                              • #45
                                Re: Pictures of process and equipment

                                hello ,i am very new to powder coating , looking to buildoven ,any info about where to find plans would be appricated ,thanks