new posts

  • Carlene
    replied
    This is my oven and spray booth. The spray booth is my old top-load wash machine. Hubby cut the back in half to make doors and riveted some side brackets on the top & bottom so I can either hang stuff off the oven rack up top or lay it on the rack on the bottom. When hanging, I just have to remember to test fit it in the oven before spraying. He put bar LED's in the front corners so I have plenty of light.

    Leave a comment:


  • autoshopowner
    replied
    and the room I shoot powder in

    Leave a comment:


  • autoshopowner
    replied
    This is my oven, an my sand blaster,
    Attached Files

    Leave a comment:


  • autoshopowner
    replied
    I screwed this post up, monitor please delete it
    Last edited by autoshopowner; 12-30-2015, 09:20 PM.

    Leave a comment:


  • driver
    replied
    Scottrods

    I left you a new post today. I do not know exactly where it went. I am sure you can find it. Computers are not my thing.
    Last edited by driver; 08-26-2013, 02:42 AM. Reason: This post is for Scottrods

    Leave a comment:


  • SCOTTRODS
    replied
    Re: Pictures of process and equipment

    Originally posted by sprayguns View Post
    Seems all pictures can't be displayed !
    Size matters, and sometimes content, if the admin is watching. Most pictures can be posted if you use photo bucket and have them sized properly.

    Leave a comment:


  • sprayguns
    replied
    Re: Pictures of process and equipment

    Seems all pictures can't be displayed !

    Leave a comment:


  • Nhoj_yelbom
    replied
    Re: Pictures of process and equipment

    Leave a comment:


  • Nhoj_yelbom
    replied
    Re: Pictures of process and equipment

    oven wtb binder


    got a hf soda blaster, works great if you have a 60+ gallon compressor. some blasted parts

    Leave a comment:


  • Nhoj_yelbom
    replied
    Re: Pictures of process and equipment

    my oven
    wtb binder

    Leave a comment:


  • KYZAAC
    replied
    Re: Pictures of process and equipment

    Originally posted by jw01247 View Post
    how do i upload pics to this site it?
    upload them to photobucket or any other image hosting site and copy the IMG tag. i'd like to see some more pics up here too

    Leave a comment:


  • jw01247
    replied
    Re: Pictures of process and equipment

    how do i upload pics to this site it?

    Leave a comment:


  • JTW37
    replied
    Re: Pictures of process and equipment

    Old thread, why not start a new one with your pics?

    Leave a comment:


  • jw01247
    replied
    Re: Pictures of process and equipment

    ive been coating for a long time but recently opened up a batch from a company that partially closed down {except my batch} i will try to send some picture do you want a begining and endding process

    Leave a comment:


  • stevedwnng
    replied
    Re: Pictures of process and equipment

    [IMG][/IMG]
    OLD BOOTH

    FUTURE BOOTH

    I'm going to use my existing fan on the new booth, (an old refrigerator) and line it with filters on the inside. Anyone have any advice or tricks?