    im in the process of getting everything ordered for my first venture into powder coating, i will be doing some scrap piece then moving up to some atv parts
    so what would anyone reccomend, i had saw some threads on this kinda but i guess i didnt know enough about it yet to get what i needed from it
    brandon

  • #2
    Black Magnum, Black Beauty, coal slag, cheap stuff (all the same thing!)

    Hemi-T

    Comment


    • #3
      Slag works great, i use only fine and very fine grit.

      Comment


      • #4
        hmmm, my supplier only carries medium B/B
        cheers

        Comment


        • #5
          Slag is cheap and blasts a nice profile. If you can find it local, use it.

          Comment