    what is the melting temp of cured powder coat for powder coat? This is my first time to write in and i just done my first valve covers yesterday.

  • #2
    generally ( because nothing specific was asked in this one) it's 410F for 10-12 minutes PMT. Check out the Tips and Tricks threads for some helpful advice for all those "newbie" questions I know you're brimming with,lol. Welcome to "da boards". If there's anything that isn't covered in the threads anywhere, don't hesitate to ask...... Russ