I coated a set of aluminum heads last night and it worked out pretty nice.
The only thing was i had to set the convection oven on like 475 just to get the heads up to 350-375 using the infared thermometer. I preheated them to the same temp. It had minimal of out gassing. Wish i could get rid of all the out gassing. I did do one at a time. Well i thought i would just share this.
Mike
The only thing was i had to set the convection oven on like 475 just to get the heads up to 350-375 using the infared thermometer. I preheated them to the same temp. It had minimal of out gassing. Wish i could get rid of all the out gassing. I did do one at a time. Well i thought i would just share this.
Mike